Make: BRUKER
Model: TS 77
- Capabilities
| Indent Tip: Berkovich |
| Load: 9000 µN [max] |
| Speed: 2.0 µN |
- Applications
The system benefits applications involving the study of:
- Indentation
- SPM Imaging
- Property Mapping
- DMA Analysis for Polymer Samples.
- Charges
| ANALYSIS NAME | UG /PG Students from Academic Institution (in INR) | Research Scholar from Academic Institution (in INR) | Project Staff from Academic Institution (in INR) | Faculty Members from Academic Institution (in INR) | Research Scientist from R&D Organizations (in INR) | Industry Personnel from Industry (in INR) | Personnel from Non – Government Organization (in INR) |
|---|---|---|---|---|---|---|---|
| Nanoindenter (maximum six indentations) | 1000 | 1000 | 1000 | 1000 | 1000 | 1000 | 1000 |
| Nanoindenter nano DMA | 1000 | 1000 | 1000 | 1000 | 1000 | 1000 | 1000 |
- Location
G02, GDN Block,
Department of Manufacturing,
Centre of Excellence in Additive Manufacturing,
School of Mechanical Engineering.
- Contact
Dr. Raja Annamalai
Dr. Vasudevan R
G02, GDN Block,
Department of Manufacturing,
Centre of Excellence in Additive Manufacturing,
School of Mechanical Engineering,
E-mail: smec.nanoindenter@vit.ac.in