Creep Testing Machine

Creep Testing Machine

Make: Applied Test Systems, USA

Model: 2330

  • Standard: ASTM E139
  • Capacity: 12000 lb
  • Temperature: 350 to 1000 o C
  • Test: Creep
    Creep Rupture
    Stress Rupture
  • Load Accuracy:+/- 0.5 %
  • Used In Aerospace, Marine, Power Plant, Nuclear, Steam Turbine Power Plants